Hi Jens,

You can try moving e0.  E0 should be on the edge.  Is E0 at the position
of the step?  You could also send us an example.  Then we can help more
directly.  I'd guess that the step is caused by some background
parameters that are set incorrectly.

SK


> -----Original Message-----
> From: ifeffit-bounces at millenia.cars.aps.anl.gov [mailto:ifeffit-
> bounces at millenia.cars.aps.anl.gov] On Behalf Of Jens Kruse
> Sent: Wednesday, January 10, 2007 8:56 AM
> To: ifeffit at millenia.cars.aps.anl.gov
> Subject: [Ifeffit] Problems with the >flatten< option in Athena
> 
> Hi,
> 
> I have a normalization problem with Athena. If I turn on the "flatten"
> option in the background removal section, Athena creates in some of
the
> normalized spectra a step in the pre-edge range.  How can I  get rid
of
> it?
> 
> Thanks,
> 
> jens
> _______________________________________________
> Ifeffit mailing list
> Ifeffit at millenia.cars.aps.anl.gov
> http://millenia.cars.aps.anl.gov/mailman/listinfo/ifeffit



More information about the Ifeffit mailing list