Hi
I have used the Athena 0.8.054 to processing the EXAFS data of Ge quantum
dots. You can find the .prj file in the attachment. In fact, they are a
seriers of samples with or without annealing at high temperature.
Surely, the data after annealing is difficult to deal with. Please do not
hesitate to give me some advices! Such as the issues on normalization,
deglitching, truncating, etc. Thanks a lot.
PS, I think this is a good way to exchange experiences and learn knowledges.
Kefan
--
Kefan Wang
School of Physics and Electronics
Henan University, 475004
E-mail: kfwang at henu.edu.cn; wang.kefan at gmail.com
-------------- next part --------------
An HTML attachment was scrubbed...
URL: <http://millenia.cars.aps.anl.gov/pipermail/ifeffit/attachments/20071217/0d1994d6/attachment.htm>
-------------- next part --------------
A non-text attachment was scrubbed...
Name: Ge QDs.prj
Type: application/x-gzip-compressed
Size: 7732 bytes
Desc: not available
URL: <http://millenia.cars.aps.anl.gov/pipermail/ifeffit/attachments/20071217/0d1994d6/attachment-0002.bin>
More information about the Ifeffit
mailing list